Perform the test on finely powdered material, and break up lumps, if necessary, with the aid of a mortar and pestle before weighing the specimen. Weigh the specimen to be tested without further treatment, unless a preliminary drying at a lower temperature, or other special pretreatment, is specified in the individual monograph. Unless other equipment is designated in the individual monograph, conduct the ignition in a suitable muffle furnace or oven that is capable of maintaining a temperature within 25

of that required for the test, and use a suitable crucible, complete with cover, previously ignited for 1 hour at the temperature specified for the test, cooled in a desiccator, and accurately weighed.